+8615958356827

Common quality problems and solutions of bottle blowing machine

Apr 27, 2022

1、 Bad shape of bottle:

a: The temperature of the whole bottle blank is too low. In this case, increase the temperature of the preform.

b: The air outlet of blow molding cavity is poor. Check whether the air outlet is blocked.

c: The pressure of blow molding air is not enough. Check the pressure of blow molding air

d: The capacity of blow molding air is not enough. Check the supply circuit of blow molding air.

2、 Wrinkled bottle surface:

a: The time of one blow molding is too late, and the preform temperature relative to this part is too low. Speed up the blow molding timer once.

b: The temperature of bottle blank is uneven. Please raise the temperature of this heater.

c: The thickness of bottle blank is uneven. Check the preform.

3、 When the bottle blowing machine is heated, the bottle blank is bent and deformed:

a: Incorrect rotation of bottle blank during heating. Confirm whether there is collision between the reflector and the like.

b: Local overheating of bottle blank. Adjust the output of the heater section.

c: The preform is too hot. Check the preform.